Superior Abrasion
Cerasol has excellent abrasion property. |
For Iron application, Cerasol sustains 50,000 cycle or 22,000m of wearing test on the iron solplate. |
For Hair Straightener, Cerasol sustains 20,000 cycle on wearing test on the heating plate. |
Main Advantages over other organic coating are summarized in the following table: |
| |
Cerasol |
Organic coating |
| Abrasion |
Super |
Relatively Poor |
| Far Infrared Ray |
Yes |
No |
| Hardness |
7H - 9H |
4H or less |
| Tourmaline |
Available |
Not Effective |
| Color |
Wide Range |
Limited / Low Gloss |
| Non-Toxic |
Yes |
No |
| Low Curing Temp |
80℃ |
280℃ - 400℃ |
| Non-Flammable |
Yes |
No |
| Non-Stick |
Yes |
Yes |
|
| Select a property to compare : |
|
|
|
|
|
|
|
|
|
| |
|